Reasons for substandard performance and
poor hardness of aluminum profile
Generally speaking, ultra-high mechanical
performance is also high hardness, mechanical performance is not qualified
corresponding to low hardness, mechanical performance is not qualified refers
to the material in the stretching process of the anti-pull strength and yield
strength does not meet the requirements;
The reason for the occurrence
1. When squeezing, the aluminum profile rod
temperature and exit temperature are not up to standard
2. The cooling speed of the profile is not
enough
3. Use the wrong stick
4. Time-caused furnace failure
Countermeasures.
1. Ensure that the process is under control
2. To ensure that the rod is not wrong, the
whole process of production in the process of standard implementation, regular
testing furnace temperature, do a good job of equipment maintenance
3. Ensure that the cooling equipment is
intact and the aluminum profile can be cooled evenly