The cause of bending during the powder coating
of aluminum profiles
The reason for the occurrence
1. Pre-treatment oil removal is not clean
2. Chrome film weight is not up to standard
3. Powder adhesion and bending performance
are poor
4. The curing temperature is not enough
Countermeasures.
1. De-oil etching amount ≥ 1g/m2, chromium
film important ≥1g/0.6-1.2gm2
2. Adjust the powder formula
3. To regularly track the actual situation
of furnace temperature, the requirements to reach 200 degrees C±10, insulation
time 10-13min, can refer to the vertical furnace temperature setting standards
for adjustment.