The cause of the bubbles in the powder coating of aluminum profile
Font size:SMB

The cause of the bubbles in the powder coating of aluminum profile

 

The reason for the occurrence

1. The powder contains volatile substances and water

2. There is moisture on the surface of aluminum

3. The film is too thick

4. The coating cure heats up too fast

 

Countermeasures:

1. Adjust the original formula of the powder

2. Pre-treatment must be dried, before entering the furnace will tilt the material at a certain angle for drip drying, visual water-free drip state, before entering the furnace

3. Reduce the film thickness and control it in the standard range

4. Adjust the furnace temperature

Updated:2020-12-11 | Return
This article keywords: